Week of November 16, 2026
Etched UTG for the 2028 foldables is a resin story, not a glass story
TrendForce reported on 6 November, citing ZDNet Korea, that Apple and Samsung are discussing a new cover window with their suppliers for the 2028 foldables: ultra-thin glass etched down to roughly 40 micrometres in th…
The combiner is moving into the lens, and the coating has to move with it
Karl Guttag published the third part of his 2026 AR year in review on 13 November, covering TDK's meta-optic mirror, the Fourier Optics metasurface and a few more radical combiners. My takeaway as a coatings supplier…
Mercedes wants LEDs inside the glass. The hard part is the glass still looking like glass
Mercedes-Benz announced on 3 November that it is developing LED display elements laminated directly into vehicle windows: mini-LEDs for large areas such as the rear window, micro-LEDs for high-resolution animations on…
Week of November 9, 2026
Mercedes wants the window to be the display. The hard part is making it disappear.
Mercedes-Benz published on 3 November a technology piece on two display concepts that put the image in the glass rather than on a screen. The first laminates LED elements into the window composite: mini LEDs in the re…
Twenty-five billion dollars of optics orders in a week, and none of it yet for the parts a small supplier makes
In the first week of November the AI optics market printed two numbers that would have been fantasy three years ago. Lumentum, reporting on 2 November, said it had won a second near-packaged or co-packaged optics awar…
Reflective waveguides are winning on physics; plastic is where the cost fight will be
Karl Guttag published the second part of his 2026 AR year-in-review on 5 November, and the headline for me is not the field-of-view numbers but the material shift underneath them. Reflective, or geometric, waveguides,…
Week of November 2, 2026
Wolfspeed wants to sell you a waveguide substrate that reflects 20% per face
Wolfspeed put out a press release on 29 October saying its transparent silicon carbide, TSiC, is now commercially available for AR waveguides, with 200 mm optical-grade substrates on offer and 300 mm in development. M…
A rollable glass screen in a dashboard is a coatings problem before it is a glass problem
The Elec reported on 26 October that Dowoo Insys, the company that has supplied ultra-thin glass for Samsung's Galaxy Z Fold since 2019, is developing a UTG cover window for rollable OLED displays in car centre inform…
The fluoropolymer makers have cleaned up their process. That does not settle the coatings question.
Syensqo stopped making C6O4 at Spinetta Marengo in October, the last fluorosurfactant it used as a processing aid for fluoropolymers, closing a phase-out it committed to in 2022. European Coatings carried the story…
Week of October 26, 2026
UTG is coming for the dashboard, and the coating question doesn't change
The Elec reported this morning that Dowoo Insys, the company that makes the ultra-thin glass for Samsung's foldables, is developing UTG cover windows for rollable OLED centre displays with a Korean automotive electron…
Transparency is the number nobody puts on the box
Karl Guttag put a number on it this week that I wish every glasses programme would print on the spec sheet: real optical see-through needs about 80 percent transparency, and the best waveguide glasses he has measured…
Co-packaged optics went from slideware to shipping in one OCP week
Three things happened at the Open Compute summit last week that tell me co-packaged optics is no longer a roadmap item. Intel said it is the only foundry with high-volume indium phosphide lasers on 300 millimetre sili…
Week of October 19, 2026
1.3 million AR glasses is both a doubling and a rounding error
How a specialty coatings company should think about a market that is growing 111% a year and is still too small to matter. TrendForce published its AR glasses forecast on 15 October. Shipments are expected to go from…
What ASML’s capacity problem tells a thin-film supplier one hour down the road
Europe’s most valuable company cannot build machines fast enough. The signal travels upstream, and it arrives at companies like ours in a very specific form. ASML reported third-quarter results on 14 October: sales o…
When the optics giant Zeiss buys the hologram startup
What Zeiss paid for when it bought Ceres Holographics was not the hologram. It was seventeen years of learning how to make one, reliably, for a car company. On 12 October Zeiss announced that it had acquired Ceres Ho…
Week of October 12, 2026
A memory maker just wrote “AR glasses” into its annual report
Micron filed its FY2026 10-K on 9 October. For the first time, the filing names smart glasses as a consumer category for its embedded memory and describes AR glasses as a driver of demand for low-power, small-form-fac…
Fifty-five years in one niche
On 7 October PPG announced a $70 million expansion of its aerospace transparencies site in Huntsville, Alabama, the plant that makes cockpit and passenger windows. The move is unglamorous: a newly leased 112,000 squar…
When the glass gets 15% dearer
Corning is raising the price of its yen-denominated display glass substrates by more than 15% from this quarter. It is the company’s first display-glass increase in over three years, and the stated reasons are familia…
Week of October 5, 2026
Decoration is becoming a functional layer
Two press releases from Kurz ahead of Fakuma, which opens in Friedrichshafen on 13 October, say more about where surface finishing is going than most conference talks. One shows contour-following roll-on hot stamping…
The $399 glasses and the €899 glasses are fighting over the same lens
Two kinds of smart glasses will be on European faces within a month, and the cheap pair tells me more about our market than the expensive one. Meta's Ray-Ban Display, with a single waveguide in the right eye, goes on…
Veldhoven just raised €40 million for a machine. The resin is the next part.
Morphotonics closed a Series B of more than €40 million on 22 September, with 3M Ventures, Innovation Industries and BOM returning, and Invest-NL, the EIC Fund, Ernij Next and a €20 million convertible from the Europe…
Week of September 28, 2026
The bottleneck in AI glasses is a piece of glass
At Meta Connect last Wednesday, Meta opened online ordering for its Ray-Ban Display glasses in the US, UK and Canada, and pre-orders in France, Italy and Germany at €899, with deliveries from 13 October. The glasses…
In a smaller company every product has to be both
Last Friday BASF confirmed it is in exploratory talks with RAG-Stiftung and Evonik about a takeover of Evonik, adding that "the course and outcome of these exploratory talks remain open at this stage." Evonik confir…
The pricing letter is the most honest document in our industry
On Friday 25 September Perstorp announced immediate global price increases on its oxo chemicals and acids, "effective immediately or as existing contracts permit", because of "sharply increasing raw material and energ…
Week of September 21, 2026
The slow part of the AR glasses
Snap launched Specs. The chip got the keynote. The coatings decide whether anyone wears them. Snap launched Specs on 16 September: 2,195 dollars, 51-degree field of view, 132 to 136 grams, four hours of battery, lens…
What a pilot plant admits
Covestro opened a recycling pilot in Leverkusen. The useful word in the press release is “pre-industrialization”. On 17 September Covestro opened a pilot plant in Leverkusen for chemical recycling of Vulkollan, the c…
The small rules arrive first - Compliance, a day job
Nothing happened on PFAS this week. Two smaller things did, and in a small company those are the work. PFAS first, because everyone asks. ECHA's risk committee gave its opinion in March, the socio-economic committee…
Week of September 14, 2026
Waveguides just became a manufacturing story. That is when materials companies matter.
Two announcements in one week say the AR optics bottleneck has moved from the lab to the line.(Finally) On 9 September, Lumus announced that Zhejiang Crystal-Optech will become the third manufacturer of its geometric…
When a supplier consolidates, the SME reads the footnote
Two quiet announcements this week, and what “supply to customers is unaffected” really means. Two announcements passed through the coatings trade press this week that most readers will have skipped. Perstorp Polyols…
The PFAS-free deadline already passed. Now comes the hard part.
What food packaging can teach optical coatings about life after fluorine. For most of my industry, the PFAS restriction is still a future event. We talk about it in the conditional: when the universal restriction com…
Week of September 7, 2026
PFAS-free" is a claim, not a virtue — the EmpCo test for specialty coatings
In three weeks, half the adjectives on our industry's datasheets become a legal liability. From 27 September the EU's Empowering Consumers Directive applies, and words like "green", "sustainable" or "eco-friendly" are…
Nanostructures on a roll- Surventis, Aumovio
When a freshly carved-out coatings giant chooses its first public partnership, it tells you where it thinks the growth is. Surventis, the former BASF Coatings, announced this week that it will develop microstructured…
European IP, Chinese scale
Every European photonics founder eventually meets the same fork. Stay small and sovereign, or hand the scaling to a partner who already has the factories and the customers, usually in Asia. TriLite in Vienna chose th…