Transparency is the number nobody puts on the box
Karl Guttag put a number on it this week that I wish every glasses programme would print on the spec sheet: real optical see-through needs about 80 percent transparency, and the best waveguide glasses he has measured get a little over 60. Birdbath designs, the ones you see in most of the cheap "AR" glasses, let about 20 percent of the world through, which makes them portable VR with a window. My view after fourteen years of coating optical stacks is that most of that missing 20 percent is not lost in the grating physics. It is lost at interfaces, one untreated surface at a time, and that part is fixable.
Count the surfaces in a display-glasses lens. Cover lens, two sides. Waveguide, two sides. A dimming layer, two more. A prescription element bonded at the factory, another two. Every bare glass-to-air surface reflects roughly 4 percent at normal incidence, more at the angles a wide field of view actually uses. Six bare surfaces is 22 percent gone before a single photon has been diffracted anywhere. You can argue about how many of those surfaces are optically bonded and therefore not air interfaces, but the ones that are not are exactly where the transparency goes.
That is also where the artefacts come from. Eye glow, the thing that makes the wearer's eye light up for everyone else, is outcoupled light leaving on the wrong side. Rainbows are stray diffraction reaching the eye through surfaces that were never meant to carry an image. Guttag lists slanted-grating artefacts as something companies are only now addressing. The common thread is that light is going places it was not invited, and in a waveguide the invitation is written by refractive index contrast. A cladding layer with an index well below the waveguide does two jobs at once: it keeps the total internal reflection honest, and it stops the grating from radiating out the back.
The nanoimprint route makes this sharper, not easier. The resin that carries the grating sits at 1.5 to 1.9 in index, and the residual layer under the structures reflects enough to eat field of view. Rokid is expected to launch full-colour AI glasses on a nanoimprinted surface-relief waveguide this week. Whoever is making those will have spent as much time on the layer under the grating and the anti-reflection on top as on the grating itself, and none of that appears in the launch video.
What customers will ask for next is not a higher-index resin. It is lower reflection per surface, a cladding that holds the waveguide at 1.2 or below without cracking at 20 microns, and all of it without fluorine, because the restriction is still on the table in Brussels. Those are coating questions, not display questions.
Transparency is not a feature you add to glasses. It is what is left after the stack has finished taking its cut.