Twenty years of precision coating science

Kriya Materials continues a nanoparticle-coating lineage that began at the Philips Physics Laboratory (NatLab), where the technology was developed and mass-produced for Philips display manufacturing from the 1990s until Philips ended display production in 2003. Kriya was founded in 2006 on Chemelot in Geleen to industrialise that technology for a broader customer base. In 2022, with Holland Capital joining as investor, we moved to our expanded facility in Nuth — with scale options for large-volume programmes.

2006

Founded on Chemelot

75+

Product codes

>10%

Of corporate budget on R&D

Innovation trajectory

From one product to a complete platform

Twenty years of compounding innovation. Each capability built on the previous — from single nanoparticles to multi-functional, multi-layer coating systems serving every major optical application.

1990s–2003

1 capabilities

Philips NatLab origins

Nanoparticle synthesis and coating technology developed and mass-produced at the Philips Physics Laboratory (NatLab) to supply Philips display manufacturing, until Philips ended display production in 2003.

RI 1.42–2.40Dispersions

2006

1 capabilities

Kriya Materials founded

Founded on Chemelot in Geleen to continue and industrialise the NatLab-developed nanoparticle coating technology for a broader customer base.

RI 1.42–1.55Hard coating

2008

2 capabilities

First OEM customer

A major Korean display manufacturer qualifies Kriya's antistatic hardcoat for plasma display panels.

RI 1.42–1.55Hard coatingAnti-static

2009

2 capabilities

Scale-up: 0 → 120 MT in one year

From zero to 120 metric tonnes of antistatic colour-filter coating delivered in a single year. Proof of manufacturing scalability.

RI 1.42–1.55Hard coatingAnti-static

2010–2014

6 capabilities

Global PDP supplier + HRI/LRI launch

Single global supplier of antistatic colour-filter coating for PDP. Launch of HRI and LRI nanoparticles for OLED enhancement. Product line expands to anti-reflection and anti-fouling.

RI 1.16–1.95Hard coatingAnti-staticHRILRIAnti-reflectionAnti-fouling

2015–2017

8 capabilities

Multi-functionality + first investors

Single coatings start combining multiple functions: anti-static + anti-fouling + hardcoat in one layer. ATO nanoparticle synthesis developed for NIR blocking. Entry into automotive thermal management. Shift Invest and Chemelot Ventures invest in 2017.

RI 1.16–1.95Hard coatingAnti-staticHRILRIAnti-reflectionAnti-fouling+1 more

2018

8 capabilities

Henkel strategic investment

Henkel invests, validating the platform approach. Accelerates R&D into UV-curable systems and 100% solids for nanoimprint lithography.

RI 1.16–1.95Hard coatingAnti-staticHRILRIAnti-reflectionAnti-fouling+1 more

2019

10 capabilities

Mass-scaled multi-functional AR coatings

Launch of mass-produced multi-functional AR coating systems. Building energy applications validated with TNO/BMC simulations across 10 cities worldwide.

RI 1.16–1.95Hard coatingAnti-staticHRILRIAnti-reflectionAnti-fouling+3 more

2020–2021

11 capabilities

Solvent UV-hybrid platform + foldable displays

New chemistry family extends RI range to 1.95 with UV-curable processing. Foldable display hardcoat passes 200,000 fold cycles, single-layer combining AS+AF+HC.

RI 1.16–1.95Hard coatingAnti-staticHRILRIAnti-reflectionAnti-fouling+4 more

2022

12 capabilities

Holland Capital + facility expansion

Holland Capital joins as lead investor. Move to expanded facility in Nuth. Capacity designed for >100,000 kg/yr dispersions, 1,000,000 kg/yr coatings.

RI 1.16–1.95Hard coatingAnti-staticHRILRIAnti-reflectionAnti-fouling+5 more

2023–2024

13 capabilities

PFAS-free AF + thermal HRI on glass + LIDAR AR

PFAS-free anti-fouling achieves WCA >100°. Thermal HRI reaches RI 1.85 with 8H hardness on glass. LIDAR-tuned AR coatings demonstrated at 905 and 1550 nm. ULR polarizer coating benchmarks against Japanese incumbents.

RI 1.16–2.00Hard coatingAnti-staticHRILRIAnti-reflectionAnti-fouling+6 more

2025–2026

15 capabilities

Full platform: RI 1.16–2.00, 75+ products

PFAS-free LRI launched down to RI 1.16. 100% solids UV-curable platform (RI 1.34–1.65) for NIL/R2R waveguide manufacturing. Solvent UV-curable LRI at RI 1.30. Platform now spans 4 chemistry families, 75+ product codes, 12+ functional capabilities.

RI 1.16–2.00Hard coatingAnti-staticHRILRIAnti-reflectionAnti-fouling+8 more

Manufacturing

From nanoparticle synthesis through dispersion formulation to final coating products, the entire value chain is controlled under one roof.

>100k kg/yr

Dispersion capacity

1M kg/yr

Coating capacity designed

0.8 μm

Batch filtration

Up to 10 CTQ

Quality parameters per batch

ISO 9001:2015 certified. Every batch filtered to 0.8 μm. 6-month guaranteed shelf life unless otherwise agreed (unopened). For large-volume programmes, back-up options are available to ensure supply security.

Download ISO 9001:2015 certificate (PDF)

Global reach

Through partners and, in selected geographies, direct local staff, Kriya serves a global customer base across Europe, Asia-Pacific and the Americas.

Want to learn more about Kriya?

Our team is available to discuss how our platform can support your application.