Photonics & Metalenses

High refractive index materials for metalens replication, diffractive optical elements, and integrated photonic circuits. Imprint-proven to n 1.79 (solvent-based UV); coatings to n 2.00. PFAS-free.

n = 1.79Imprint-proven refractive index
$3.1B*Metalens market by 2032
<50 nmTypical nanoparticle size
R2RManufacturing scale

Metalens replication

Flat optics at R2R production scale

Metalenses replace curved glass optics with flat nanostructured surfaces. They require high refractive index materials that can be structured — by imprint or as coated layers. Kriya’s solvent-based UV resist with n 1.79 at 633 nm was nano-imprinted in peer-reviewed work; the same family is available as a coating up to n 1.95, and the broader platform reaches n 2.00 for overcoat and index-matching layers.

Metalens: RI 1.16-2.00

Various chemistry families and curing technologies. NIL-compatible for sub-wavelength nanopillar structures.

Both thermal and UV-curable

Thermal variants 130-350 deg C. UV variants enable sub-second cure for high-throughput NIL replication.

n = 1.00Air (optical path)n = 1.79 imprint-proven; up to 1.95 evaluationKriya HRI metalens layersolvent-based UVn = 1.65-1.85Kriya HRI planarisation layerTiO2 nanon = 1.52Glass / polymer substraten = 1.30-1.40Kriya LRI AR coatingKM-005n = 1.00Air (backside)
Metalens optical stack — Kriya HRI for nanopillar replication, HRI planarisation, and LRI backside AR
Metalens optical stack — Kriya HRI for nanopillar replication, HRI planarisation, and LRI backside AR
LayerRefractive indexKriya materialProduct
Air (optical path)1.00NoN/A
Kriya HRI metalens layer1.79 imprint-proven; up to 1.95 evaluationYessolvent-based UV
Kriya HRI planarisation layer1.65-1.85YesTiO2 nano
Glass / polymer substrate1.52NoN/A
Kriya LRI AR coating1.30-1.40YesKM-005
Air (backside)1.00NoN/A

Integrated photonics

Beyond Moore: light replaces electrons

On-chip photonic interconnects, optical neural networks for AI acceleration, and photonic qubits for quantum computing all require materials with precisely controlled refractive indices. Kriya’s RI 1.16 to 2.00 platform provides the complete materials toolkit for integrated photonics.

Light guiding

Optical waveguides and light management using precisely controlled RI materials

LiDAR on chip

Solid-state beam steering via photonic integrated circuits

n = 1.30-1.40Kriya LRI cladding (top)100% solidsn = 1.85-2.00Kriya HRI waveguide coreUV-curen = 1.30-1.40Kriya LRI cladding (bottom)100% solidsn = 1.46SiO2 / SOI substrate
On-chip photonic waveguide — Kriya HRI core with LRI cladding provides the RI contrast needed for light confinement
On-chip photonic waveguide — Kriya HRI core with LRI cladding provides the RI contrast needed for light confinement
LayerRefractive indexKriya materialProduct
Kriya LRI cladding (top)1.30-1.40Yes100% solids
Kriya HRI waveguide core1.85-2.00YesUV-cure
Kriya LRI cladding (bottom)1.30-1.40Yes100% solids
SiO2 / SOI substrate1.46NoN/A

Diffractive optical elements

Precise RI control for every optical layer

Diffractive optics, holograms, and beam-shaping elements all depend on controlled RI gradients. Kriya’s four chemistry families — sol-gel, UV-curable solids, UV-curable hybrids, and thermal-curable latex — provide the formulation flexibility to hit any RI target from 1.16 to 2.00 with the processing characteristics each application demands.

Sol-gel

1.16-2.00

200-700 deg C cure. Spin, dip, roll, spray. Low-outgassing grades available.

100% solids UV

1.34-1.65

Solvent-free. R2R and NIL compatible. Screen printing.

Solvent UV hybrids

1.30-1.95

Multi-layer AR stacks. Gravure, slot die, dip, float, spin.

Thermal latex

1.36-1.50

Versatile. Co-solvent thermal cure. Nearly any known application method.

Market context

$3.1B*

Global metalens market forecast for 2032. Driven by smartphone cameras, automotive sensors, and medical devices.

$16B

Global optical coatings market. Photonics represents the highest-growth segment within this space.

2026+

Kriya roadmap: extending 100% solids to <1.37 RI and >1.60 RI for expanded photonics applications.

* Source: industry analyst estimates for metalens market size. Figures cited for contextual reference only.

Developing a photonic or metalens device?

Our R&D team brings deep nanoparticle synthesis and optical coating expertise to every project.

Start a technical discussion