← Back to all notes
R

Roel Huis in ‘t Veld

Director, Kriya Materials · Week of September 21, 2026

The slow part of the AR glasses

Snap launched Specs. The chip got the keynote. The coatings decide whether anyone wears them. Snap launched Specs on 16 September: 2,195 dollars, 51-degree field of view, 132 to 136 grams, four hours of battery, lenses that tint in ten seconds, shipping this autumn in the US, UK and France. The same two days, MicroLED Connect and AR/VR Connect ran in Eindhoven, an hour from our lab. Meta, Google and Sony on the keynote list. Lumus, Vuzix, Optinvent and Cellid for waveguides. Applied Materials, EV Group, Morphotonics and Eulitha for making them in volume. I read both programmes as a parts list. A pair of AR glasses is a waveguide with a nanostructured grating, an anti-reflective coating on each face, a tint layer, an anti-fingerprint layer, and an adhesive that must hold the waveguide without pulling the light out of it. Every one of those is a coating. The projector and the chip get the stage. The layers decide the weight, the price and whether the thing survives a summer in a glovebox. Take the weight. Normal sunglasses weigh about thirty grams. Specs weigh 132. The difference is glass versus polymer and refractive index versus thickness. Field of view scales with the index of the waveguide material. Glass gets you to 1.9 or 2.0. Polymers stop around 1.7 and move when they get warm. Optinvent showed a moulded polymer waveguide in Eindhoven. Whether that works is a materials question, and materials questions take about two years to answer. That is my point. Compute, AI and sensors follow exponential curves. Optical materials do not. They follow qualification clocks: adhesion, haze at oblique angles, 500 hours at 65 degrees and 85 percent humidity. A reliability test cannot be sped up. So the convergence everyone is waiting for runs at the speed of its slowest component, and that component is a coating. We work at both ends of the index scale, high-index layers so a waveguide can be thinner and layers near 1.2 that keep the light inside the glass where glue or frame would let it out. Neither is glamorous. Both take a year at a customer before a single gram ships. Meta Connect is on 23 and 24 September. Ignore the field of view. Watch the price and the weight, because that is where the materials budget shows. Nobody knows the AR volumes for 2029. What I know is that qualification starts three years before volume. The specifications being written this month are the real news. The launch only proved the stack works at 136 grams and 2,195 dollars. Now it has to work at half of both. Sources Spatial Insider, 17 Sept 2026 – Snap Specs launch — https://spatialinsiders.com/stories/snap-specs-launch-highlights-september-2026 Snap Inc. – Specs optics and lens details — https://investor.snap.com/news/news-details/2026/Snap-Inc--Debuts-SPECS-Augmented-Reality-Glasses-to-Make-Computing-More-Human/default.aspx MicroLED-Info – MicroLED Connect 2026 programme — https://www.microled-info.com/glimpse-microled-connect-2026-waveguides-optics-and-road-mass-market-ai-glasses Road to VR – Meta Connect 23–24 September — https://roadtovr.com/meta-connect-2026-date-announcement/