← Back to all notes
R

Roel Huis in ‘t Veld

Director, Kriya Materials · Week of November 16, 2026

Etched UTG for the 2028 foldables is a resin story, not a glass story

TrendForce reported on 6 November, citing ZDNet Korea, that Apple and Samsung are discussing a new cover window with their suppliers for the 2028 foldables: ultra-thin glass etched down to roughly 40 micrometres in the folding strip and left thicker than 100 micrometres everywhere else, with the groove filled by a material that must match the glass optically. DigiTimes carried the story on 12 November, and TechRepublic adds that a decision is expected in the fourth quarter of 2027. Everybody writes this up as a glass breakthrough. It is the opposite. The glass part is known, the filler is the whole problem, and the filler is a coating. Today's foldables use uniform UTG: 45 micrometres on the iPhone Duo and the Galaxy Z Fold8 Ultra, 60 on the Z Fold8 and 50 on the Z Flip8, according to TrendForce. Uniform means compromise: thick enough not to dent under a fingernail, thin enough to survive hundreds of thousands of folds. Etching only the hinge strip lets you have both, on paper. But you now have a groove some 60 micrometres deep, as wide as the hinge zone, to fill flush with a material that does not scatter, show an edge, creep or crack when the glass bends. What matching the glass really means: refractive index to within about 0.005 at 550 nanometres, or you see a step at the sidewalls; matching dispersion, or you see a faint coloured line; and matching how the index drifts with temperature, because an acrylate changes index by about one part in ten thousand per degree while glass barely moves, so a perfect match at room temperature is 0.003 off in a trouser pocket in summer. On top of that, acrylates shrink several percent on cure. Fill a 60 micrometre groove in one go and you get a two or three micrometre dip unless you stage the cure or formulate for low shrinkage, and that is visible under a window. Then the mechanics. A filler of two to three gigapascal modulus next to glass at seventy is a stiffness step of roughly 25 to 1, right where the panel bends. Stress concentrates at the resin edge, which is where delamination starts. Whoever formulates this is designing a gradient: a low-shrink, index-matched core with adhesion to etched glass, a hard skin that takes the usual hard-coat and anti-fingerprint stack, and a thermal response that tracks the glass over the life of the phone. What coating flexible substrates since 2012 has taught me is that index matching is the easy half and ageing is the hard half. Yellowing after UV, index drift after moisture uptake and micro-cracks after thermal cycling all show up at the one place a customer looks first, the crease. The supplier that gets picked in late 2027 will be the one with a filled coupon still invisible after a thousand hours of damp heat, not the one with the thinnest etch. If the 2028 foldable looks flat, it will be because a resin chemist did their job and nobody noticed. Sources TrendForce, “[News] Samsung, Apple Reportedly Eye Stronger Foldable Displays with Etched Ultra-Thin Glass by 2028”, 6 November 2026. https://www.trendforce.com/news/2026/11/06/news-samsung-apple-reportedly-eye-stronger-foldable-displays-with-etched-ultra-thin-glass-by-2028/ DigiTimes, “Apple, Samsung reportedly developing new foldable glass for 2028”, 12 November 2026. https://www.digitimes.com/news/a20261112VL206/apple-samsung-foldable-2028-utg.html TechRepublic, “Foldable Glass Gets a Redesign: What Apple and Samsung Are Testing”, 12 November 2026. https://www.techrepublic.com/article/news-apple-samsung-foldable-glass-2028/