R
Roel Huis in ‘t Veld
Director, Kriya Materials · Week of October 5, 2026
The $399 glasses and the €899 glasses are fighting over the same lens
Two kinds of smart glasses will be on European faces within a month, and the cheap pair tells me more about our market than the expensive one. Meta's Ray-Ban Display, with a single waveguide in the right eye, goes on sale in Germany, France and Italy on 13 October at €899. Samsung's Android XR glasses, built with Warby Parker and Gentle Monster and without any display, are now reported to be launching next month at around $399. Both are sold as eyewear, and for a coatings company that is the point: the lens is where the money is decided, not the chip.
Take the cheap pair first. There is no waveguide, no microdisplay, no optical engine. What is left is a lens that has to be light, anti-reflective, anti-fouling, often prescription, and that will be handled, wiped and dropped far more than a normal pair of glasses because it is also a camera and a headset. That is a coatings product sold as fashion. The brands that make these frames have spent a century learning how to sell a lens; they have spent about three years learning that the lens now has to survive a product cycle instead of a season.
Now the expensive pair. A waveguide only works because of what surrounds it. The low-index layers, the protective stack, the anti-reflection on both faces and the lens it is bonded to decide whether the image is crisp or washed out, and whether the glasses look like glasses or like lab equipment. Whoever supplies those layers is in the eyewear business whether they like it or not. I find that a useful way to think, because it stops us from treating AR as a niche. It is a lens with extra steps.
Then there is the supply side. Digitimes reported last week that Chinese panel makers are ramping Micro OLED capacity for smart glasses before the demand is proven. I have seen this film before, in displays and in solar: capacity arrives early, prices fall, and the component that was supposed to be scarce becomes a commodity within two years. When that happens the differentiation moves outward, to the optics and the surfaces, because that is what the customer actually sees and touches.
For a specialty materials company like ours this is both the opportunity and the warning. The opportunity is obvious: every one of these lenses needs coatings that did not exist in volume five years ago, and the big eyewear groups are only now building the capability to specify them and thus knocking on our door from every corner of the world for our PFAS free imprintable layers.
The warning is that the volumes will come from Asia first, through the frame makers and the waveguide foundries, not through the brand in Milan, Singapore, Seoul or Menlo Park. If you want to be in the lens, you need to be in that supply chain before the $399 pair becomes the $199 pair.
My bet is that within three years the question "what coating is on it" will matter more to the consumer's experience than "which processor is in it". We build for that.