R
Roel Huis in ‘t Veld
Director, Kriya Materials · Week of November 2, 2026
The fluoropolymer makers have cleaned up their process. That does not settle the coatings question.
Syensqo stopped making C6O4 at Spinetta Marengo in October, the last fluorosurfactant it used as a processing aid for fluoropolymers, closing a phase-out it committed to in 2022.
European Coatings carried the story on 30 October: nearly 100% of its fluoropolymers are now made without PFAS processing aids, with about 1% of the site's volume, specialised grades for hydrogen and semiconductor uses, still to be qualified on existing C6O4 stock.
Good news. But let me be clear about what it does and does not change for anyone making optical coatings.
What it changes is the argument about emissions. The processing aids are the small, mobile PFAS molecules, the part of fluoropolymer production that regulators and the communities around the plants have been most concerned about. Taking them out of the process is the strongest card the fluoropolymer industry has in the universal PFAS restriction that is still under evaluation in Brussels. Syensqo's CEO Mike Radossich said as much in Hydrocarbon Processing on 28 October: fluoropolymers remain essential materials for the energy transition. Expect that line in every submission on the derogations.
What it does not change is where the fluorine sits in an optical coating. In an anti-reflective stack on a cover lens the low-index layer does the work, and the cheap way to get a polymer below an index of 1.40 is to fluorinate it. The anti-fingerprint layer on top is typically a fluorinated silane with a perfluoropolyether tail. Neither is a processing aid. They are the product, they sit on the surface, and they wear off under a thumb. A cleaner polymerisation route changes none of that.
The second piece of news makes the point from the regulatory side. European Coatings reported on 13 October that the PFHxA restriction, Entry 79 of REACH Annex XVII, took effect on 10 October for consumer mixtures, textiles, footwear, food-contact paper and cosmetics, with limits of 25 parts per billion for PFHxA and its salts and 1,000 ppb for related substances in homogeneous material. The article is careful to say this is not a universal ban on PFAS in industrial coatings, which is right. But the related-substances clause is the one that catches the C6 fluorotelomer chemistry a lot of the surface-treatment industry moved to after it left C8, and 25 ppb is a detection-level number. Once a compliance team has seen that figure in one category, it asks for it in all of them.
That is what I see in practice. The question in RFQs is no longer whether the coating complies, it is whether it contains any organofluorine at all. The alternative route to low index is porosity rather than fluorine: hollow or nanoporous silica, index 1.20 to 1.39, which does the optics well and then has to be made hard enough to survive a wipe test, which is where the development effort goes.
The industry has cleaned up how it makes fluoropolymers; the market has already decided it would rather not have them on the glass.
Sources
European Coatings, “Syensqo Ends PFAS Fluorosurfactant Production in Italy”, 30 October 2026. https://www.european-coatings.com/news/markets-companies/syensqo-ends-pfas-fluorosurfactant-production-in-italy/
Hydrocarbon Processing, “Syensqo ends fluorosurfactant production at Italian site”, 28 October 2026. https://hydrocarbonprocessing.com/news/2026/10/syensqo-ends-fluorosurfactant-production-at-italian-site/
European Coatings, “EU PFHxA Restrictions Under REACH Now in Effect”, 13 October 2026. https://www.european-coatings.com/news/markets-companies/eu-pfhxa-restrictions-under-reach-now-in-effect/