Illuminated laminated glazing

Why laminating with a near-index interlayer kills guiding — and how a low-index cladding restores it.

Lessons

  1. Lesson 1
    The edge-lit laminated stack

    Glass, cladding, interlayer, glass — four index steps.

    ~7 min read
  2. Lesson 2
    Why an index-matched interlayer lets light escape

    No TIR when n_PVB ≈ n_glass.

    ~7 min read
  3. Lesson 3
    A low-index cladding restores guiding

    Thin, low-n, high-contrast — the three requirements.

    ~7 min read
  4. Lesson 4
    A logo as an extraction pattern

    A rasterised binary pattern multiplied into the brightness map.

    ~7 min read
  5. Lesson 5
    Uniformity and halo

    What a clean halo looks like and what a bad one does.

    ~7 min read

References

  • Hecht, E. Optics, 5th ed. (Pearson, 2017). §4.7 — Total internal reflection and the evanescent wave.
  • Zhu, S. et al. Frustrated total internal reflection in a prism-pair interferometer. Journal of Modern Optics 61, 1104 (2014).
  • Jackson, J. D. Classical Electrodynamics, 3rd ed. (Wiley, 1998). §7.4 — Reflection and refraction with dielectric interfaces.
  • Wu, C. & Narimanov, E. E. Analysis of a passive illuminated-glazing architecture. Optics Express 24, 11130 (2016).

Further exploration — related tools

  • title— Edge-lit plate brightness-map render — see hot spots dissolve as Kriya cladding widens the TIR acceptance cone
  • title— Edge-lit light guide: ray propagation, extraction features, luminance uniformity
  • title— θ_c, escape/guided fraction, evanescent depth, min cladding thickness