A halo is the faint light bleeding beyond the intended extraction pattern — the designed logo appears sharp, and a soft glow surrounds it at reduced brightness. Depending on cladding quality and extraction-pattern tuning, the halo can be a feature or a defect.
A good halo
- Brightness falls off smoothly from the pattern edge over 20–40 mm.
- Colour is uniform (no yellow / blue cast).
- No visible ring at the plate edge where injection sits.
A bad halo
- Bright arc at the injection edge: too little guided fraction — raise cladding thickness or lower cladding index.
- Blue cast in the halo: short-λ frustrated TIR leaks more than long; cladding is too thin.
- Dark cross-stripes: the extraction pattern is interfering with the LED geometry; reposition LEDs or re-tune the pattern density gradient.
What the tool helps you decide
It quantifies both — overall uniformity score and halo fall-off slope — so you can trade cladding thickness, extraction pattern, and LED current against a single pass / fail on the final visual spec.