Illuminated panoramic roofs are laminated glass stacks: outer glass, interlayer, inner glass. To make them edge-illuminable, insert a thin low-index cladding between the glass and the interlayer — the stack becomes glass / cladding / interlayer / glass, and the TIR calculation lives at the glass / cladding interface.
Four index steps
A typical architecture:
- Outer glass: n = 1.52
- Cladding: n ≈ 1.20, ~200 nm thick
- Interlayer (PVB or similar): n = 1.48
- Inner glass: n = 1.52
LEDs sit in the glass edge and inject into the outer plate. Guided rays bounce along; a patterned extraction surface turns some of them out as controlled illumination.
Low-refractive-index coatings down to RI 1.16, overcoatable and PFAS-free, live on the low-refractive-index-coatings technology page.