Three short tasks in the Illuminated Panoramic Roof. Each one gives you the inputs; you report the number.
This tool doesn’t accept URL parameters, so the “Open in tool” buttons below open the tool at its landing page. Set the inputs listed in each exercise by hand.
Glass / PVB — guided fraction without a cladding
Quantify the TIR collapse when glass is laminated directly to PVB.
Inputs to set
n_plate: 1.52 (glass)
n_outside: 1.48 (PVB)
Return guided fraction (%)
Open in tool ↗Open the Illuminated Panoramic Roof tool. Set up a 1.52 glass plate with PVB (n = 1.48) on both faces, no cladding. Record the guided fraction.
Glass + cladding — guided fraction restored
Add the low-index cladding and compare.
Inputs to set
n_plate: 1.52 (glass)
n_cladding: 1.20
Return guided fraction (%)
Open in tool ↗Insert a 1.20 cladding between the glass and the PVB on both faces. Record the guided fraction.
Minimum cladding thickness at ε = 1 %
Compute the thinnest cladding that keeps per-bounce frustrated-TIR leak into the PVB below 1 % at a 60° bounce.
Inputs to set
n_plate = 1.52
n_cladding = 1.20
n_beyond = 1.48
angle = 60°
λ = 550 nm
Open in tool ↗Set n_plate = 1.52, n_cladding = 1.20, n_beyond = 1.48, angle = 60°, λ = 550 nm, max leak = 0.01. Record d_min.