Making low index

Mixing rules for composite coatings, porous films, and hollow-sphere nanoparticles — the bridge from material fractions to an effective index.

Lessons

  1. Lesson 1
    Volume fractions and mixing

    How bulk fraction maps to an effective optical response.

    ~7 min read
  2. Lesson 2
    Maxwell-Garnett

    Dilute inclusions in a host; where the formula applies and breaks.

    ~9 min read
  3. Lesson 3
    Bruggeman

    Symmetric EMA for roughly equal phases, with a self-consistency step.

    ~8 min read
  4. Lesson 4
    Lorentz-Lorenz and choosing the rule

    Additive polarisabilities, and a pragmatic model-selection heuristic.

    ~7 min read
  5. Lesson 5
    Porous coatings and hollow nanoparticles

    Two-step EMA for hollow spheres; link to the LRI Particle Engineering Model.

    ~10 min read
  6. Lesson 6
    Why d ≪ λ — the haze limit

    Rayleigh scattering, particle size, and the transparency budget.

    ~8 min read

References

  • Maxwell Garnett, J. C. "Colours in metal glasses and in metallic films." Phil. Trans. R. Soc. A, 203, 385–420 (1904).
  • Bruggeman, D. A. G. "Berechnung verschiedener physikalischer Konstanten von heterogenen Substanzen." Ann. Phys. (Leipzig) 24, 636–664 (1935).
  • Bohren, C. F. & Huffman, D. R. Absorption and Scattering of Light by Small Particles (Wiley, 1998). §8.5 on effective media.
  • Macleod, H. A. Thin-Film Optical Filters, 4th ed. (CRC, 2010). Ch. 8 — porous films.
  • Kriya Validation Cases — Effective Medium regression set.

Further exploration — related tools

  • title— Hollow-sphere geometry → RI via two-level Maxwell-Garnett effective medium
  • title— Mie 1908 exact solution — Qext/Qsca/Qabs/g for dielectric spheres, Beer-Lambert through filled layer
  • title— Transfer Matrix Method — R(λ), T(λ), A(λ) for multilayer stacks