Practice test
Eight questions, instant feedback, unlimited retries. Score ≥ 7.0 / 10 to count the module as passed.
- Question 1
Why does an effective-medium approximation require particle size much smaller than the wavelength?
- Question 2
Maxwell-Garnett mixing: 15% air in a 1.52 host.
- n_host = 1.52
- n_inclusion = 1.00
- f = 0.15
- Question 3
For which configuration is Maxwell-Garnett (host + dilute inclusions) most appropriate?
- Question 4
Bruggeman mixing: 50% air, 50% silica (n = 1.46).
- Rule: Bruggeman
- Phase 1 n = 1.46 (SiO₂)
- Phase 2 n = 1.00 (air)
- f = 0.50
- Question 5
Lorentz-Lorenz mixing: 40% air in a 1.50 binder.
- Rule: Lorentz-Lorenz
- Binder n = 1.50
- Air n = 1.00
- f = 0.40
- Question 6
Effective index of a hollow silica particle: 100 nm outer diameter, 15 nm shell.
- Outer Ø = 100 nm
- Shell = 15 nm
- Shell n = 1.46
- Core n = 1.00
- Question 7
Why can a porous coating reach refractive indices below any solid material’s index?
- Question 8
Rayleigh scattering intensity scales as: