Porous coatings and hollow nanoparticles

Two-step EMA for hollow spheres; link to the LRI Particle Engineering Model.

Lesson 5 of 6 · ~10 min read

To reach the low indices a broadband AR design wants (n ≈ 1.2–1.3), you must beat the lowest-index solid dielectrics (MgF2 is the industry’s cheap limit at 1.38). The only route is a porous coating — adding air to a solid at a sub-wavelength scale.

Two paths to porosity

  1. Inter-particle voids. Pack dense solid nanoparticles with gaps between them. Classic sol-gel silica sits here.
  2. Intra-particle voids. Each nanoparticle is itself a hollow shell. The void lives inside the particle; the film can be denser overall and still have a lot of air.

Two-step EMA for hollow-sphere coatings

The Effective Medium Calculator models a Kriya-style LRI coating in two steps:

nparticle = MG(nshell, ncore, fvoid)
(2.5.1)
ncoating = mix(nbinder, nparticle, fparticle)
(2.5.2)

For a thin-shell silica sphere with outer diameter 80 nm and 10 nm shell, the void fraction is 1 − (1 − 2·10/80)3 ≈ 0.578, and nparticle ≈ 1.21. Packing those into a binder at 60% volume fraction drops the coating index into the 1.2–1.3 range.