Coating colour and rainbow

From a reflectance spectrum to CIELAB, ΔE2000 across angle, and the rainbow index for thickness variation.

Lessons

  1. Lesson 1
    From R(λ) to XYZ to L*a*b*

    The CIE pipeline as the tool implements it: CMFs, illuminant SPD, 5-nm integration.

    ~9 min read
  2. Lesson 2
    Why residual reflection has colour

    A V-shape in R(λ) is not neutral grey.

    ~7 min read
  3. Lesson 3
    Angle shift and ΔE2000

    The five preset angles, CIEDE2000 by Sharma et al., and how to read the plot.

    ~9 min read
  4. Lesson 4
    Thickness variation and the rainbow index

    Why a ±5 nm wet-coating drift reads as rainbow.

    ~7 min read
  5. Lesson 5
    Trading mean R for neutral colour

    The two-knob design trade: push mean R down, push ΔE up.

    ~7 min read

References

  • CIE 15:2018 — Colorimetry, 4th ed. (Commission Internationale de l'Éclairage, 2018).
  • Sharma, G., Wu, W. & Dalal, E. N. "The CIEDE2000 Color-Difference Formula." Color Res. Appl. 30, 21–30 (2005).
  • Wyszecki, G. & Stiles, W. S. Color Science, 2nd ed. (Wiley, 1982).
  • Kriya Validation Cases — Colour-shift regression set.

Further exploration — related tools

  • title— Transfer Matrix Method — R(λ), T(λ), A(λ) for multilayer stacks
  • title— Differential evolution optimiser over TMM forward model
  • title— Physically rendered ghost reflection of a lit scene on a coated surface — angle, colour and brightness from the TMM kernel