Hands-on exercises

Three short tasks in the Colour-Shift / Rainbow Index. Each one gives you the inputs; you report the number.

This tool doesn’t accept URL parameters, so the “Open in tool” buttons below open the tool at its landing page. Set the inputs listed in each exercise by hand.

Read the b* of the MgF₂ reference stack

Open the Colour-Shift calculator and load the single-layer MgF₂ reference stack. The tool runs the CIE 1931 2° observer against the D65 SPD at 5-nm steps on the TMM-kernel reflectance.

Inputs to set
  • Coating layer: MgF₂, n = 1.38, d = 99.6 nm.
  • Substrate: ns = 1.52 (BK7 glass).
  • Illuminant D65, CIE 1931 2°, evaluate at 0°.
Open in tool ↗Report the CIELAB b* coordinate of the normal-incidence reflected colour under D65 to two decimals.

Angle shift on a MgF₂ single-layer AR

Same MgF₂ reference stack. The tool evaluates R(λ) at 0°, 15°, 30°, 45° and 60°, runs the CIE pipeline at each and reports CIEDE2000 relative to normal incidence.

Inputs to set
  • Coating layer: MgF₂, n = 1.38, d = 99.6 nm.
  • Substrate: ns = 1.52.
  • Illuminant D65, CIE 1931 2°.
  • Compare reflected Lab at 0° and 45°; apply CIEDE2000 per Sharma et al. (2005).
Open in tool ↗Report ΔE2000 between 0° and 45° to one decimal.

Angle shift on a 1.16-index single-layer AR

Swap the coating layer for a low-index film at n = 1.16, d = 118.5 nm on the same glass. The lower top-layer index drives the quarter-wave null deeper and narrower, which also makes the residual colour and its angle drift larger.

Inputs to set
  • Coating layer: n = 1.16, d = 118.5 nm.
  • Substrate: ns = 1.52.
  • Illuminant D65, CIE 1931 2°.
  • Compare reflected Lab at 0° and 45°; apply CIEDE2000 per Sharma et al. (2005).
Open in tool ↗Report ΔE2000 between 0° and 45° to one decimal.