Broadband AR stack optimisation

Merit functions, quarter-wave starts, layer indices and the differential-evolution search the optimiser actually runs.

Lessons

  1. Lesson 1
    The merit function and the wavelength band

    What the optimiser actually minimises and why the mean-R objective makes a broadband stack.

    ~8 min read
  2. Lesson 2
    Quarter-wave starts vs optimised thicknesses

    Why λ₀/4 is the historical starting point and how DE pushes past it.

    ~7 min read
  3. Lesson 3
    Choosing indices and why a very low top layer widens the band

    Index contrast as the broadband lever; the 1.16 top layer worked example.

    ~9 min read
  4. Lesson 4
    Differential evolution and Nelder-Mead polish as implemented

    DE/rand/1, F=0.8, CR=0.7, pop 15–30, Nelder-Mead polish — line by line.

    ~10 min read
  5. Lesson 5
    The substrate back side and practical limits

    How the back-surface correction enters, and why wet coating caps layer count and thickness.

    ~8 min read

References

  • Macleod, H. A. Thin-Film Optical Filters, 4th ed. (CRC Press, 2010). Ch. 3: "Anti-reflection coatings".
  • Storn, R. & Price, K. "Differential Evolution." J. Global Optim. 11, 341–359 (1997).
  • Nelder, J. A. & Mead, R. "A Simplex Method for Function Minimization." Comput. J. 7, 308–313 (1965).
  • Kriya Validation Cases — AR optimiser regression set.

Further exploration — related tools

  • title— Transfer Matrix Method — R(λ), T(λ), A(λ) for multilayer stacks
  • title— CIE 1976 u'v' rainbow index, ΔE₀₀ across angle set
  • title— Manufacturing-tolerance Monte Carlo — ±σ bands, worst-case, yield-at-spec