Three short tasks in the Broadband AR Stack Optimizer. Each one gives you the inputs; you report the number.
This tool doesn’t accept URL parameters, so the “Open in tool” buttons below open the tool at its landing page. Set the inputs listed in each exercise by hand.
Match the MgF₂ textbook baseline
The classic single-layer AR on glass is a quarter-wave of MgF₂ at 550 nm. Reproduce its band-averaged reflectance in the optimiser and confirm the number matches the TMM Simulator.
Inputs to set
Substrate: Glass (BK7)
Back surface: black-backed
Layer 1: MgF₂ (n = 1.38), d = 99.6 nm
Target band: 450–650 nm
Open in tool ↗Open /tools/ar-optimizer. Set the substrate to Glass (BK7), back surface to black-backed, target band to 450–650 nm. Do NOT run the optimiser — instead, set one layer, material MgF₂, thickness 99.6 nm, and read the mean R directly from the spectrum. Report the mean R.
Low index wins the band
Swap MgF₂ for a Kriya LRI 1.16 layer at the same quarter-wave design and read the mean reflectance. The index is near the √(n_0·n_s) match, so the broadband curve should collapse almost to zero.
Inputs to set
Substrate: Glass (BK7)
Back surface: black-backed
Layer 1: Kriya LRI 1.16, d = 118.5 nm
Target band: 450–650 nm
Open in tool ↗Same setup as Exercise 1 — substrate BK7, black-backed, band 450–650 nm. Change Layer 1 to Kriya LRI 1.16 at 118.5 nm. Do not run the optimiser; just read the mean R.
A diagnostic two-layer stack
Add a half-wave high-index layer underneath the 1.16 quarter-wave. A half-wave is an "absentee" at the design wavelength — it contributes nothing at 550 nm but reshapes the broadband curve. Does it help?
Open in tool ↗Build a two-layer stack on BK7 black-backed. Layer 1 (top): Kriya LRI 1.16, 118.5 nm. Layer 2 (next to substrate): Kriya HRI 1.95, 141.0 nm. Band 450–650 nm. Read the mean R, no optimiser run.