Practice test
Eight questions, instant feedback, unlimited retries. Score ≥ 7.0 / 10 to count the module as passed.
- Question 1
What does the AR Stack Optimizer actually minimise when the objective is set to "minimise reflectance"?
- Question 2
Load the tool with a single 99.6 nm layer of MgF₂ (n = 1.38) on BK7 glass. Target band 450–650 nm, back surface set to black-backed. What is the mean reflectance?
- Substrate: Glass (BK7), back surface black-backed
- Layer 1: MgF₂ (n = 1.38), thickness 99.6 nm
- Band: 450–650 nm
% - Question 3
A quarter-wave single-layer AR on BK7 at 550 nm reaches a theoretical zero when the layer index equals which value?
- Question 4
Replace the MgF₂ with a Kriya LRI layer at n = 1.16, d = 118.5 nm on the same BK7 substrate, black-backed. Target band 450–650 nm. Mean reflectance?
- Substrate: Glass (BK7), back surface black-backed
- Layer 1: Kriya LRI 1.16, thickness 118.5 nm
- Band: 450–650 nm
% - Question 5
The AR Optimizer uses differential evolution. Which parameters does it run with?
- Question 6
For the same MgF₂ quarter-wave stack (n = 1.38, d = 99.6 nm) on BK7 black-backed, what is the reflectance exactly at 550 nm?
- Substrate: Glass (BK7), back surface black-backed
- Layer 1: MgF₂ (n = 1.38), d = 99.6 nm
- Read at a single wavelength: 550 nm
% - Question 7
Stack: n = 1.16, d = 118.5 nm on top of n = 1.95, d = 141.0 nm, on BK7 glass, black-backed. Target band 450–650 nm. Mean reflectance?
- Substrate: Glass (BK7), back surface black-backed
- Layer 1 (top): Kriya LRI 1.16, 118.5 nm
- Layer 2 (next to substrate): Kriya HRI 1.95, 141.0 nm
- Band: 450–650 nm
% - Question 8
Why does the optimiser hand the DE winner to a Nelder-Mead simplex instead of stopping at the DE result?