Envelope-method metrology

Swanepoel 1983: fringes, envelopes, n(λ), k(λ), and thickness from a single T spectrum.

Lessons

  1. Lesson 1
    Fringes and the Airy formula

    Where the sinusoid in T(λ) comes from.

    ~7 min read
  2. Lesson 2
    Upper and lower envelopes

    Smooth maxima and minima — the method's first move.

    ~7 min read
  3. Lesson 3
    Cauchy fit and the conjugate-root ambiguity

    Two n(λ) branches for a low-index film, broken by an ellipsometry anchor.

    ~9 min read
  4. Lesson 4
    Thickness from the interference phase

    Counting fringes and bisecting d.

    ~7 min read
  5. Lesson 5
    When the method breaks

    Too thin, too absorbing, non-uniform — and how to see it in the data.

    ~7 min read

References

  • Swanepoel, R. Determination of the thickness and optical constants of amorphous silicon. Journal of Physics E: Scientific Instruments 16, 1214 (1983).
  • Manifacier, J. C., Gasiot, J. & Fillard, J. P. A simple method for the determination of the optical constants n, k and the thickness of a weakly absorbing thin film. Journal of Physics E 9, 1002 (1976).
  • Cauchy, A. L. Mémoire sur la dispersion de la lumière. Prague (1836).
  • Macleod, H. A. Thin-Film Optical Filters, 4th ed. (CRC Press, 2010). Ch. 9: "Measurement of thin-film properties".
  • González-Leal, J. M. et al. The use of the Swanepoel method for obtaining the optical constants of thin films. Thin Solid Films 517, 2110 (2009).

Further exploration — related tools

  • title— Cauchy + Urbach dispersion fit to Ψ, Δ; single- or multi-angle
  • title— Transfer Matrix Method — R(λ), T(λ), A(λ) for multilayer stacks
  • title— Composite & porous coating index from constituents and volume fraction.