Hands-on exercises

Three short tasks in the Swanepoel Envelope Analyzer. Each one gives you the inputs; you report the number.

This tool doesn’t accept URL parameters, so the “Open in tool” buttons below open the tool at its landing page. Set the inputs listed in each exercise by hand.

Substrate index from Ts

Compute the substrate refractive index from a bare transmittance measurement, Swanepoel eq. (2).

Inputs to set
  • Ts: 0.918
  • Formula: s = 1/Ts + √(1/Ts² − 1)
  • Enter s
Open in tool ↗Open Swanepoel. Enter a bare-substrate transmittance of Ts = 0.918. Read the substrate index.

Film index in the HRI regime

Read n at one extremum for a high-index film from a single (TM, Tm, s) triple.

Inputs to set
  • TM: 0.93
  • Tm: 0.60
  • s: 1.52
  • Regime: HRI (n > s)
Open in tool ↗Enter TM = 0.93, Tm = 0.60, s = 1.52. Use Swanepoel eq. (9): N = 2s(TM−Tm)/(TM·Tm) + (s² + 1)/2, then n² = N + √(N² − s²).

Thickness from an extremum pair

Compute film thickness from two consecutive maxima using Swanepoel eq. (13).

Inputs to set
  • λ₁: 500 nm
  • n₁: 2.00
  • λ₂: 700 nm
  • n₂: 1.95
  • Formula: Swanepoel eq. (13)
Open in tool ↗Two maxima: λ₁ = 500 nm with n₁ = 2.00, λ₂ = 700 nm with n₂ = 1.95. Apply d = λ₁λ₂ / [2(n₁λ₂ − n₂λ₁)].