Upper and lower envelopes

Smooth maxima and minima — the method's first move.

Lesson 2 of 5 · ~7 min read

Swanepoel's first step: separate T(λ) into a smooth upper envelope TM(λ) through the maxima and a smooth lower envelope Tm(λ) through the minima. The tool fits splines (or uses PCHIP) through the extrema to get continuous envelopes across the whole spectrum.

The job those envelopes do

  • Every wavelength now has a (TM, Tm) pair, not just the measured extrema.
  • The pair at any λ captures the fringe amplitude and so the local reflectance product R12·R23, which is what n(λ) inversion needs.
  • The substrate transmittance Ts(λ) — measured separately — gives s(λ) through Swanepoel eq. (2).

Why smooth envelopes, not just extrema

Measured T is discrete. If you invert only at the extrema you get one n per fringe, not a continuous n(λ). The envelopes carry the fringe information across the whole band so the Cauchy fit (next lesson) has enough points.