Yellowing Prediction

How much will this coating yellow under UV exposure?

Bracket long-term Δb* yellowing for a substrate and stabiliser strategy.

How it works

Polymer coatings yellow when UV photons break chemical bonds and produce chromophores that absorb at the short-wavelength end of the visible band. The accumulated absorbance at a reference wavelength scales with the total UV dose and the material's susceptibility. The perceptual shift is quantified by the b* coordinate in a uniform colour space.

Worked example

Yellowness Δb* = k · t^n (ASTM G154 cycle)

Fit against three internal weathering datasets.

Validation method, references and test-case results: /validation#yellowing

Request accessOpen the interactive tool