Yellowing Prediction

Bracket long-term Δb* yellowing for a substrate and stabiliser strategy.

Validation: hand-checked example → /validation#yellowing

Inputs are substrate (PC kLow 0.030 / kHigh 0.070, PET 0.008 / 0.020, PMMA 0.003 / 0.008, TAC 0.015 / 0.035, Glass 0.0005 / 0.002 — provisional Xenon-arc ranges), exposure site (South Florida 275 MJ/m²/yr, Arizona 335, Central Europe 115, Northern Europe 75, Tropical 250, Custom), duration in years, stabiliser package (None 1.0 / UV 0.5 / HALS 0.7 / UV+HALS 0.35 for PMMA, substrate-dependent), and duty cycle %. Dose basis is broadband 300–400 nm total UV per ASTM G7-20. Computes dose = irradiance_avg × duty/100 × years × 31 536 kJ/m² and Δb* = k × stab × √dose. Validity range 0–2500 MJ/m² (Wypych §3 fit); beyond that the UI warns.