Cure Shrinkage Calculator
How much does this resin shrink on cure?
Estimate dry-film thickness, volumetric loss, and density-increase factor from cure shrinkage of the chosen chemistry family.
How it works
A curing resin shrinks as its monomers polymerise into a denser network. The shrinkage fraction depends on the monomer chemistry and the achieved degree of cure. The induced residual stress adds to any thermal-mismatch stress in the finished coating.
Worked example
UV acrylate, 5 % volume shrinkage, 10 µm wet film
Constrained-film cure shrinkage: all volume loss projected into thickness.
Validation method, references and test-case results: /validation#cure-shrinkage