Cure Shrinkage Calculator
Estimate dry-film thickness, volumetric loss, and density-increase factor from cure shrinkage of the chosen chemistry family.
Validation: hand-checked example → /validation#cure-shrinkage
Wet films contract during cure — sol-gel networks 10–15%, hybrids 5–10%, UV-curable acrylates 5–10%, 100%-solids UV acrylates 5–15% (brief Group 5, 2026-11: ~22.5 cm³/mol per reacted C=C per Odian 4th ed. Table 3-5). The calculator takes wet film thickness, volume solids (%) and chemistry family (which auto-fills a typical shrinkage you can override), and returns the dry thickness, volume lost, and the density-increase factor implied by mass conservation. Formula: dry = wet × (solids/100) × (1 − s/100). Useful before locking a slot-die gap or Mayer bar number.