Energy, buildings & agriculture

Crystalline-silicon PV module

Front glass that lets more light in and stays clean

About 4 % of the sunlight hitting a module bounces off its front glass before it reaches the cells. A porous low-index layer cuts that reflection; an anti-soiling top coat helps keep dust from eating the gain back.

SUNBACKAnti-soiling top coatOuter faceLow-index anti-reflection layerPorous, PFAS-freeSolar glass3.2 mm · n 1.52EncapsulantEVA or POE · n ≈ 1.48Silicon cells and ribbonsNot KriyaEncapsulantNot KriyaBacksheet or rear glassNot KriyaK1K2
Kriya coating position — published on kriya-materials.comKriya chemistry applies — application fit from public literatureOther device layers — not supplied by Kriya
All layers (7)
  1. Anti-soiling top coat Outer faceK1
  2. Low-index anti-reflection layer Porous, PFAS-freeK2
  3. Solar glass 3.2 mm · n 1.52
  4. Encapsulant EVA or POE · n ≈ 1.48
  5. Silicon cells and ribbons Not Kriya
  6. Encapsulant Not Kriya
  7. Backsheet or rear glass Not Kriya

Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.