Displays & wearables

LCD with LED backlight

Monitor, notebook and TV panel

An LCD shapes light from the backlight between two polarizers. Kriya chemistry sits on the polarizer films — where hard coat, low reflection and antistatic decide contrast, durability and touch performance — and can keep light guided when backlight films are bonded together instead of stacked with air gaps.

VIEWER SIDEBACKLIGHTSurface treatment on the frontpolarizerHard coat + low-reflection AR (anti-glareoption)Front polarizerTAC / PVA / TAC · n ≈ 1.48–1.50Pressure-sensitive adhesiveNot KriyaColour-filter glassn 1.52Liquid crystaln ≈ 1.5–1.7TFT array glassn 1.52Rear polarizerTAC / PVA / TACAntistatic hard coatOn the rear polarizer filmReflective polarizer filmRecycles the blocked polarizationPrism filmsBrightness enhancementDiffuser filmNot KriyaLow-index layer for bonded backlightfilmsReplaces the air gap above the light guideLight-guide plate with edge LEDsPMMA (n 1.49) or glass · printed extractiondotsReflector filmNot KriyaK1K2K3
Kriya coating position — published on kriya-materials.comKriya chemistry applies — application fit from public literatureOther device layers — not supplied by Kriya
All layers (14)
  1. Surface treatment on the front polarizer Hard coat + low-reflection AR (anti-glare option)K1
  2. Front polarizer TAC / PVA / TAC · n ≈ 1.48–1.50
  3. Pressure-sensitive adhesive Not Kriya
  4. Colour-filter glass n 1.52
  5. Liquid crystal n ≈ 1.5–1.7
  6. TFT array glass n 1.52
  7. Rear polarizer TAC / PVA / TAC
  8. Antistatic hard coat On the rear polarizer filmK2
  9. Reflective polarizer film Recycles the blocked polarization
  10. Prism films Brightness enhancement
  11. Diffuser film Not Kriya
  12. Low-index layer for bonded backlight films Replaces the air gap above the light guideK3
  13. Light-guide plate with edge LEDs PMMA (n 1.49) or glass · printed extraction dots
  14. Reflector film Not Kriya

Public references

  1. US 6,210,858 — Anti-reflection film and display device using the same — 1997 filing: wet-coated anti-reflection film with hard coat, high-index layer and a low-index layer (n 1.20–1.55) that owes its index to micro voids
  2. US 5,834,549 — Transparent conductive coating composition and transparent antistatic molded article — 1998 patent: UV-curable transparent coating made antistatic with conductive tin-oxide powder, for substrates such as polycarbonate
  3. US 6,742,921 — Light pipe, plate light source unit and reflection type liquid-crystal display device — 2000 priority: a layer bonded to a light guide through a lower-index layer, so that guided light is totally reflected at the interface

Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.