Displays & wearables
Foldable OLED display
Smartphone cover window and display stack
A foldable phone cannot use rigid cover glass. Its cover is a thin polyimide (CPI) or PET film, often over ultra-thin glass, and that cover must carry hardness, anti-reflection and easy-clean in layers that survive folding many times a day. Wet nanocomposite coatings stay flexible where brittle sputtered stacks crack.
Kriya coating position — published on kriya-materials.comKriya chemistry applies — application fit from public literatureOther device layers — not supplied by Kriya
All layers (13)
- Easy-clean topcoat Fluorine-free, hollow-silica based · n ≈ 1.40K1
- Anti-reflection layers High-index + low-index stack · n 1.16–1.95K2
- Foldable hard coat UV-cured nanocomposite on the cover filmK3
- Cover film Colourless polyimide (CPI) or PET · cover window 30–200 µm
- Optically clear adhesive Not Kriya
- Ultra-thin glass (in UTG designs) ≈ 30–70 µm
- Optically clear adhesive Not Kriya
- Circular polarizer Suppresses ambient reflection from the metal electrodes
- Touch sensor Metal mesh, on-cell
- Thin-film encapsulation Inorganic/organic barrier
- OLED emitters Red, green, blue subpixels · organic layers n ≈ 1.7–1.9
- TFT backplane on polyimide LTPS / LTPO
- Back film and support plate Not Kriya
Public references
- G.-M. Choi et al., Flexible Hard Coating: Glass-Like Wear Resistant, Yet Plastic-Like Compliant, Transparent Protective Coating for Foldable Displays — Adv. Mater. 29, 1700205 (2017): a hard coating on plastic film for the cover window of foldable displays
More on kriya-materials.com
- kriya-materials.com/applications/displays
- kriya-materials.com/applications/displays/foldable-display-hardcoat
- kriya-materials.com/case-studies/foldable-display-hardcoat
Kriya tools used on this page
Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.