Flat optics & imaging
Smartphone camera
Cover window, wafer-level optics and image sensor
Light reaches each pixel through a cover window, a lens stack, an IR-cut filter and a microlens. Light bouncing between the cover window and the lens stack shows up as flare and ghosts; inside the sensor, index steps decide how much light each pixel collects and how much leaks to its neighbours.
Kriya coating position — published on kriya-materials.comKriya chemistry applies — application fit from public literatureOther device layers — not supplied by Kriya
All layers (9)
- Easy-clean / AR, outer face Exposed to fingers and pocketsK1
- Camera cover window Glass (n ≈ 1.5), sapphire (1.77) or PC (1.58)
- Anti-reflection, inner face Protected side of the windowK1
- Lens stack Molded aspheres or wafer-level replicated lensesK2
- IR-cut filter Not Kriya
- Microlens array One lens per pixel · n ≈ 1.6
- Low-index grid / planarisation Between microlenses and colour filtersK3
- Colour filters Bayer mosaic
- Silicon photodiodes Not Kriya
Public references
- H. A. Macleod, Thin-Film Optical Filters, 3rd edition (2001), chapter 3: Antireflection coatings — multi-layer designs for the visible; sections 3.4 and 3.5: coatings with two zeros, and coatings for the visible and the infrared together · link: publisher page of the current edition
- C. C. Fesenmaier, Y. Huo, P. B. Catrysse, Optical confinement methods for continued scaling of CMOS image sensor pixels — Opt. Express 16, 20457 (2008), open access: three ways to guide light from the microlens to the photodiode, one of them a low-index cladding, compared on optical efficiency and crosstalk
More on kriya-materials.com
Kriya tools used on this page
Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.