Two- and three-layer anti-reflection

V-coat, W-coat, broadband trade-offs.

Lesson 5 of 6 · ~9 min read

One quarter-wave gives you one narrow zero at the design wavelength. Two layers give you two tunable parameters and a V-shape. Three layers give you a plateau. The industry’s broadband AR coatings are stacks of 5–9 layers.

Two layers — the V-coat

One quarter-wave high-index film on top of one half-wave low-index film (or vice versa) can be designed to hit zero at a target wavelength with a sharper notch than a single quarter-wave. The second layer buys an extra phase lever, at the cost of narrower bandwidth.

Three layers — the W-coat and broadband AR

A three-layer AR with carefully chosen (n, d) at each level can hit two reflectance minima within the visible band — the W-shape — giving <1% average reflectance from 400–700 nm.

Why low-index matters here too

The top layer wants to be as close to n0 as possible, and the whole stack’s bandwidth widens as the lowest n available drops. Sub-1.3 porous low-index films — like Kriya LRI 1.16 to 1.30 — unlock single-layer designs with wider bands and multi-layer designs with less material.