Substrates and the back-side correction

How the simulator treats the second interface, and when it matters.

Lesson 4 of 6 · ~7 min read

The characteristic-matrix reflectance treats the substrate as semi-infinite. The light that transmits into the substrate goes to zero at depth with no second interface. Real substrates have a back surface, and real measurements see the back-surface reflection too.

How the TMM Simulator treats the back surface

Two scenarios:

  • Opaque substrate (k > 0, e.g. silicon in the UV). The forward wave is absorbed before reaching the back; the back surface is irrelevant. The simulator reports T = 0 and lumps the absorbed power into A. This keeps R + T + A = 1 by construction.
  • Transparent substrate (k ≈ 0, e.g. BK7). The simulator’s R is the front-surface coherent reflectance only. For a measured total you add the incoherent back-surface reflectance separately. For a 1 mm glass slab that back reflection is typically ~4%; broadband-AR comparisons report "front-surface only" to avoid double counting.