Efficiency vs uniformity

The two numbers that trade against each other in every LGP.

Lesson 2 of 5 · ~7 min read

Add more extraction features and the plate gets brighter near the edge but uniformity drops (the far end runs out of rays). Space them farther apart and uniformity improves but total output falls. The design space is a Pareto frontier between the two.

Two dimensionless metrics

  • Extraction efficiency η = fraction of edge-injected flux that emerges through the top face. Typical range 60–85 %.
  • Uniformity U = 100 · min(top-face luminance) / max(top-face luminance). Target range 85–97 % for backlight-grade LGPs.

Why both rise together with a low-index cladding

A low-index cladding raises the TIR cone from ~41° (against air) to ~52° (against n = 1.20). More rays stay guided, so the guided-fraction attenuation curve is flatter, so the extraction pattern needed to hit 95 % uniformity can also run at higher total efficiency. The usual trade shifts outward along the frontier.