Material choices: PMMA, glass, PC

Index, dispersion, scatter, and cost.

Lesson 3 of 5 · ~7 min read

LGP substrates are chosen for low absorption, low internal scatter, flat dispersion, and mouldability. Three materials dominate.

PMMA — the default

  • Index n = 1.49 at 550 nm.
  • Low internal haze (sub-0.5 % per cm), low Abbe number, cheap, easily moulded at 220 – 240 °C.
  • TIR against air gives θc ≈ 42.2°; guided fraction ≈ 74.4 %.

Glass — when thinness matters

  • Index n = 1.52 at 550 nm.
  • Stiffer than PMMA; practical plates go thinner for the same mechanical spec. Higher raw-material cost, chip-sensitive.
  • TIR against air: θc ≈ 41.1°; guided fraction ≈ 75.4 %.

Polycarbonate (PC) — impact resistance

  • Index n = 1.586 at 550 nm.
  • Higher internal scatter than PMMA, more absorption in the blue. Chosen where impact or heat is the real constraint.