Extraction features: dots vs prisms

Two mechanisms that outcouple TIR-trapped light.

Lesson 1 of 5 · ~8 min read

A feature on the back surface of an LGP breaks the TIR condition locally — the ray hits a facet at an angle below the critical angle and transmits. Two canonical shapes do this: diffuse dots and prisms.

Printed dots (diffuse)

A white-pigment or beads-in-binder dot scatters incoming rays into a wide Lambertian cone. A fraction emerges below the critical angle and escapes through the top face. Pros: isotropic output, easy to grade spatially. Cons: lower efficiency per hit (most rays scatter back into TIR), gentle luminance roll-off.

Moulded prisms (directed)

A moulded micro-prism redirects the specular ray into the escape cone with high efficiency. Pros: ~10–20 % higher luminance than dots at the same feature count; sharper viewing-angle control. Cons: angle-selective (the prism geometry works only for a range of incidence angles), harder to pattern densely without moiré.

When each wins

  • Notebook / monitor backlights: prisms, because a few extra per-cent of efficiency compound across battery life.
  • Architectural lighting: dots, because viewing directions are diverse and the prism specular hotspot would show as glare.
  • Illuminated signage: dots, often with a top diffuser to smear the dot pattern.