Designing a laminated light guide

How a Kriya LRI layer lifts guided fraction in a practical stack.

Lesson 5 of 5 · ~8 min read

Put the four pieces of the module together — critical angle, guided fraction, evanescent field, frustrated TIR — and a design workflow for a laminated light guide falls out.

Design steps

  1. Core index. Pick the highest practical ncore. More index contrast means a tighter escape cone and more guided light.
  2. Cladding index. Pick the lowest practical nclad. The guided fraction cos θc rises monotonically as nclad/ncore falls. A Kriya LRI 1.20 cladding on a 1.85 HRI core delivers θc ≈ 40.4° vs. 32.7° for bare air — moving 80% of the escape cone into TIR.
  3. Cladding thickness. From Eq. 4.4.2, size the cladding to a leak budget and expected angle range. 500 nm to 1 μm is a comfortable zone for visible wavelengths and 1% leak budgets.
  4. Validate against measured. The TIR & Escape-Cone Calculator’s methods panel cites measured regressions for the lossy modes; the LGP Simulator handles finite-length extractor patterns and real sources.

Where the physics meets the materials

The scientific limit on guided fraction is set by what nclad you can achieve as a defect-free, scalable coating. The engineering limit is usually manufacturability: solvent, cure, lamination, adhesion. Every low-index step is a linearity jump in guided fraction. That is why the laminated-waveguide community has been chasing low-index coatings for a decade.