For an isotropic source inside a planar slab of index n1, the fraction of rays that hit the top (or bottom) face inside the escape cone is
per face, so the fraction trapped by TIR at that face is cos θc (the complementary band of angles). For a slab bounded above and below by the same lower-index medium, light trapped at the top can still escape at the bottom; the full guided fraction depends on geometry (edge-fed sheet vs. isotropic point source).
Why the formula is simple
An isotropic source emits uniformly over 4π steradians. The escape cone is a spherical cap of half-angle θc; its area on the unit sphere is 2π(1 − cos θc), and there are two such caps (top and bottom). Dividing by 4π gives the formula.
Reference numbers (single face)
- PMMA → air: cos(42.1°) ≈ 0.741, so 74.1% trapped at one face.
- GaN → air: cos(24.0°) ≈ 0.914, so 91.4% trapped at one face.
- HRI → LRI (1.85/1.20): cos(40.4°) ≈ 0.762 — a higher guided fraction than HRI alone would trap against air (1.85 → air traps 87%, but the next stack layer up matters).