The evanescent field and penetration depth

What "total" in TIR actually means at nanometre scales.

Lesson 3 of 5 · ~9 min read

"Total" in TIR describes the far-field power balance, not the near-field picture. The boundary conditions still require continuous tangential fields, so a real electromagnetic field exists on the other side of the interface — it simply decays exponentially into the lower-index medium.

E(z) ∝ exp(−z / dp), with dp = λ / (2π √((n1 sin θ)2 − n22))
(4.3.1)

dp is the 1/e penetration depth. At 550 nm and 60° incidence on a glass → air TIR, dp ≈ 135 nm — comparable to a visible wavelength.

What the evanescent field does and does not do

  • It stores energy. Field energy density is non-zero on the other side; a time-averaged real field exists.
  • It does not transport power in the far field. The normal component of the time-averaged Poynting vector is zero away from the interface.
  • It couples to objects nearby. If something within a few dp breaks the exponential decay — a second interface, a scatterer — real power flows. That is Lesson 4.