Critical angle and the escape cone

The two angles that matter — and where their wedge goes.

Lesson 1 of 5 · ~7 min read

When light tries to leave a higher-index medium for a lower-index one and the angle of incidence exceeds the critical angle θc, the refracted beam vanishes. All the power stays with the reflected wave (plus an evanescent field we meet in Lesson 3).

θc = arcsin(n2 / n1), (n1 > n2)
(4.1.1)

The escape cone

Pivot the question: a light source inside the higher-index medium can only exit through the cone of angles up to θc. Everything outside that cone — in solid-angle terms, 2π(1 − cos θc) steradians per face — is trapped by TIR.

Reference numbers

  • PMMA (1.4915) → air: θc ≈ 42.1°.
  • PC (1.585) → air: θc ≈ 39.1°.
  • BK7 (1.517) → air: θc ≈ 41.3°.
  • GaN (2.45) → air: θc ≈ 24.0° — very narrow escape cone, big extraction challenge.
  • 1.85 HRI → 1.20 LRI laminate: θc ≈ 40.4° — a low-index laminate widens the trapping cone.