Packing and process porosity

The 0.74 soft cap, and a third Bruggeman stage for burn-out voids.

Lesson 3 of 5 · ~7 min read

Random close packing of identical spheres sits around 64 % by volume; face-centred cubic reaches 74.0 %. The 0.74 cap on f in step 2 is a geometric soft limit, not a physical hard one: at higher f the particles jam into each other and the "dilute host" picture breaks.

A third stage for burn-out porosity

Even when f maxes out, films made with a volatile organic binder can lose mass during cure and open up extra voids between particles. The tool models this with an optional third stage that treats the already-filled coating as a host with an additional air fraction pproc:

f · (εair − εeff) / (εair + 2εeff) + (1 − f) · (εhost − εeff) / (εhost + 2εeff) = 0

That is the Bruggeman symmetric equation. Symmetric mixing is right at high air fractions where neither phase is dilute.

Sanity checks

  • All three rules — Maxwell-Garnett, Bruggeman and Lorentz-Lorenz — agree within ~0.01 in n for air fractions below ~0.5. The rule choice is only load-bearing above that.
  • Overall air fraction (particle + coating + process) tops out below 1.0 by construction: each stage blends toward air but never equals it.
  • A pure air layer is n = 1.0. No EMA will drop below that — any model that suggests otherwise is being extrapolated beyond its regime.