Inverse design by bisection

Hit a target n_eff by solving for volume fraction.

Lesson 4 of 5 · ~7 min read

Design often runs the other way: "I need ncoat = 1.25 at 550 nm for a quarter-wave anti-reflection layer on a 1.52 substrate. What volume fraction of my hollow particles do I need in this binder?"

Monotonic in f

For a given particle and binder, the two-stage MG result ncoat(f) is monotonically decreasing in f as long as nparticle < nbinder (which is the only case that makes sense here). Monotonic plus continuous ⇒ bisection converges in O(log 1/ε) steps.

Bracketing

Start with flo = 0 and fhi = 0.74 (or the user's cap). Evaluate ncoat at both ends. If the target lies outside the bracket, the design is infeasible with the chosen particle and binder — the right fix is a smaller/hollower particle, a lower-index binder, or process porosity, not a higher f.

Tolerance

A 10⁻⁴ tolerance on n converges in ~14 bisections for the usual range. Index-matching the AR quarter-wave only needs 10⁻² (the two-layer stack is tolerant to a few % in n); go deeper only if you are trying to split hairs about colour at angle.