Levenberg-Marquardt (LM, Marquardt 1963) interpolates between gradient descent and Gauss-Newton via a damping parameter. It converges locally and quickly — provided it starts in the right basin of attraction.
The cost landscape has valleys
The Ψ cost is a smooth bowl. The Δ cost has a periodic structure in d (every half-wavelength shift in optical thickness looks almost identical in Δ), so the full cost has secondary minima one order apart. A single LM run from the wrong order ends up in the wrong basin and declares victory at a nearby local minimum.
Multistart
Launch LM from a grid of (A, d) starting guesses — typically 3×5 = 15 starts — and keep the lowest-cost converged result. If two starts converge to indistinguishable costs at different d, surface the ambiguity. Do not pick arbitrarily.
cos(Δ) vs Δ
Δ wraps at 2π. Fitting (Ψ, cos(Δ)) instead of (Ψ, Δ) avoids the discontinuity at Δ = ±π. The information content is the same for non-chiral samples; the numerics are much better.