Treat the internal rays as isotropic over the Snell-limited solid angle. The direction cosine along the plate normal, k_z, is uniform on [−1, +1]. A ray is TIR-guided when |k_z| < Kc, where Kc = cos θc.
The identity
Integrating the solid-angle element across the TIR cone (and summing the two half-spaces that contribute) gives the closed form the tool evaluates:
guided fraction = (2/π) · [ Kc · √(1 − Kc²) + arcsin(Kc) ]
With Kc = √(1 − (noutside/nplate)²), this is a one-line calculation. For a 1.52 glass plate:
- Air outside (n = 1.00): Kc ≈ 0.753 → guided fraction ≈ 75.4 %.
- PVB outside (n = 1.48): Kc ≈ 0.228 → guided fraction ≈ 22.6 % — the laminate kills the TIR budget.
- Low-index cladding (n = 1.20): Kc ≈ 0.613 → guided fraction ≈ 62.9 % — recovers most of the loss.