Frustrated TIR through the cladding

exp(−2κd) per bounce — the finite-cladding tunnelling term.

Lesson 3 of 5 · ~8 min read

A cladding thicker than ~500 nm behaves like infinite cladding for the TIR calculation — the evanescent field falls off so fast that nothing on the far side matters. Thin claddings leak.

The evanescent decay

κ = (2π/λ) · √( (nplate sin θ)² − nclad² )

The field in the cladding falls as exp(−κz). The leaked intensity on the far side of a cladding of thickness d scales as exp(−2κd) per bounce.

Solving for a minimum thickness

Set a target leak fraction ε and invert:

dmin(ε) = ln(1/ε) / (2κ)

For nplate = 1.52, bounce angle 60°, nclad = 1.20, λ = 550 nm, a ε = 1 % cap needs dmin ≈ 115 nm. Ten times tighter (1 ‰) needs ~170 nm. The dependence on ε is logarithmic — tightening the cap costs very little extra thickness.

Low-refractive-index coatings down to RI 1.16, overcoatable and PFAS-free, live on the low-refractive-index-coatings technology page.