Edge-injected Lambertian light under TIR

How a 3-D Lambertian source enters a plate with a critical angle.

Lesson 1 of 5 · ~8 min read

Edge-lit means a bright-source LED array sits at one edge of a transparent plate and fires into it. Each LED is Lambertian — its intensity falls as cos θ off the normal — and the plate's edge sees a hemisphere of directions.

What reaches the inside

Snell's law maps the external hemisphere to an internal cone around the plate normal of half-angle θt = arcsin(1/n). For n = 1.52 that is ~41°. Light inside the plate is cos-weighted and trapped inside that cone — a smaller angular spread than the external hemisphere, more directed down the plate.

Why TIR matters

Any ray inside the plate that hits the top or bottom interface at an angle steeper than the critical angle gets totally internally reflected. The internal critical angle depends on what is on the other side of the interface:

θc = arcsin(noutside / nplate)

Against air: θc ≈ 41.1° for nplate = 1.52. Against a low-index cladding at n = 1.20: θc ≈ 52.1°. Against PVB at n = 1.48 (near-matched): θc ≈ 76.9° — a very narrow TIR cone, so most rays leak straight into the PVB.

Low-refractive-index coatings down to RI 1.16, overcoatable and PFAS-free, live on the low-refractive-index-coatings technology page.