TMM Thin-Film Reflectance Simulator
How do I design or analyse a thin-film optical stack?
Compute reflectance and transmittance of an arbitrary multilayer optical stack using the characteristic-matrix (transfer-matrix) method.
How it works
The transfer-matrix method describes propagation of light through a stack of parallel homogeneous layers by multiplying a two-by-two characteristic matrix per layer. Each matrix captures the layer's phase thickness and admittance, derived from its refractive index and physical thickness. Combining the per-layer matrices gives the stack's amplitude reflection and transmission coefficients at any wavelength and angle.
Worked example
BK7 Sellmeier at 550 nm
Inputs: wavelength = 550
Result: 1.519
Reference: Schott BK7 datasheet (DL-5-82) via Macleod 5th ed. app. 3
Computed by this tool's kernel at build (commit dae6663).
Validation method, references and test-case results: /validation#tmm