All products
KM-105Available PFAS-free
Thermal LRI
Thermal-curable low refractive index coating reaching RI 1.16. Overcoatable and PFAS-free. Survives tempering at 630°C on glass. Delivers up to 3.9% transmission gain and 4.5× light guiding luminance improvement.
Refractive index rangen = 1.16–1.40
1.162.00
Chemistry familySolvent sol-gel
Cure typeThermal
Product blockKM-101–140
Specifications
Functions
Low RIAnti-reflective
Compatible substrates
GlassPET
Processing methods
SPINDIPSPRAY
Refractive index range
1.16–1.40
1.162.00
| Property | Value |
|---|---|
| Product code | KM-105 |
| Chemistry family | Solvent sol-gel |
| Refractive index range | 1.16–1.40 |
| Cure type | Thermal |
| PFAS status | Available PFAS-free |
| Functions | Low RI, Anti-reflective |
| Compatible substrates | Glass, PET |
| Processing | SPIN, DIP, SPRAY |
| Product block | KM-101–140 |
| Batch sizes | From 40 kg sample to production scale |
| Shelf life | 6 months (unopened) |
| Quality | ISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch. |
Request a sample
Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.