OLED and LED Lights – Low Refractive index
Kriya’s Low Refractive Index (LRI) coating is a solvent based, inorganic, thermal curable coating with a refractive index (RI) as low as 1.30 for glass. For plastic, it is a solvent based, organic/inorganic, UV curable coating. It can be used in optical stacks to match the RI requirements in that specific construction. Combination with a hard coat or Antistatic hard coat as a base layer is possible and results in additional mechanical and/or antistatic properties. The LRI coating can be applied by standard wet coating techniques such as gravure and slot die.
| Type | PET | TAC | PC | PMMA | Glass |
|---|---|---|---|---|---|
| Organic | Min 1.30 | Min 1.30 | Min 1.30 | Min 1.30 | |
| Inorganic | Min 1.30 |
0 = Standard | X = Optional additional feature
| Type | Scratch resistance | Overcoatable | Chemical resistance | Anti static | Near Infra Red |
|---|---|---|---|---|---|
| Organic | 0 | X | X | X | |
| Inorganic | 0 | X | X | X |
0 = Standard | X = Optional additional feature
Kriya Materials if needed develops custom formulations meeting the most stringent requirements of our customers. The result is a plug and play product designed for optimal performance at the lowest total system cost.
Please contact us through submitting our intake form.
Coatings for other substrates can be requested @ Kriya Materials
Disclaimer; Performance may depend on specific subtrate of choice, and process conditions, for each customer a customer specific product is formulated.