RI Platform Explorer
Explore the widest PFAS-free refractive index range from a single supplier
1.50n
1.162.00
Refractive index 1.50. 4 chemistry families. 2 matching products. Applications: Display AR coatings, Automotive optics.
Chemistry families
Solvent sol-gel1.16 – 2.00
Spin, dip, roll, spray
100% solids UV-curable1.34 – 1.65
R2R, NIL, screen printing
Solvent UV-curable hybrids1.35 – 1.95
Gravure, slot die, dip, float, spin
Thermal-curable latex1.36 – 1.50
Nearly any known application
Regulatory filter
Matching products
KM-040
n 1.35 – 1.95Multi-layer AR
KM-101
n 1.50 – 1.53Antistatic HC
Applications
Display AR coatingsAutomotive optics
Reflectance curve
Polymer RI varies with crystallinity (PET 1.57–1.66, PC 1.58–1.59). Defaults are Kriya consensus values; use Custom for your measured n.
Min. reflectance
3.74%
Avg. R (380–750 nm)
3.78%
At wavelength
490 nm
Reflected colour
Substrate
Glass (BK7) (n=1.518)
Transfer Matrix Method (TMM) for quarter-wave single-layer coating at normal incidence. Substrate RI includes Cauchy dispersion. Actual Kriya multi-layer products achieve broadband R < 0.15%.